info@toyar-yori.com
Molybdenum & molybdenum alloy rod

Molybdenum & molybdenum alloy rod

  1. Specification
     1)We produce pure and lanthanum doped molybdenum alloy rod;
     2)Molybdenum rod can be divided into 2 kinds: Forging molybdenum rod allows to have oxidized film and slight forging hammer mark; the surface of polished molybdenum rod presents metallic luster and has no-oxidized phenomenon notably; the two surfaces have no defects, such as divided layer, crackle, burr and vertical crackle, etc.
     3)Molybdenum rod is manufactured in random length pieces or cut to customers' desired lengths with diameters ranging from 0.20 inches to 1.75 inches.


 2. Features:
 1).The density of our molybdenum rods from 9.8g/cm3 to 10.1g/cm3; The smaller diameter is,the density is higher.
 2).Its purity is higher than 99.95%;
 3).Molybdenum rod possesses features with high hot hardness, high thermal conductivity, and low thermal expansion to hot work steels;
 4).It is a silvery-white, hard, transition metal, which has the eighth-highest melting point of any element;
 5).Molybdenum rod burns only at temperatures above 600 °C (1,112 °F);
 6).It has the lowest heating expansion of any commercially used metal.

3.Product Description

Product Name

Factory direct supply molybdenum metal bar sintered on sale

Material

Molybdenum alloy or Pure molybdenum

Dimensions

Dia. 1-300mm length ≤ 2000mm

Surface Treatment

Forging, Squeezing, Sintering

Package

Carton box, wooden case or as request

Service Project

To provide production design, production and technical service, mould development and processing, etc.

MOQ

2 pcs

Delivery

10-15 working days

Payment

Paypal, wire-transfer, L/C, D/A, D/P, T/T, Western Union, MoneyGram, Other

Application

Molybdenum electrode, Molybdenum boat, Crucible vacuum furnace, Nuclear energy etc.

The specification would be changed by the customers' requirements.

  1. Comparison between alloy molybdenum and pure molybdenum

Physical properties

Material

Density/g·cm-3

Melting point/℃

Boiling point/℃

TZM alloy(Ti0.5/Zr0.1)

10.22

2617

4612

Mo

10.29

2610

5560

TZM alloy (molybdenum zirconium titanium alloy) (Ti0.5/Zr0.08)
 Mechanical properties

Mechanical properties

Elongation/%

Elastic Modulus/GPa

Yield Strength/MPa

Tensile strength/MPa

Fracture toughness

/(MP·m1/2)

Numerical value

<20

320

560~1150

685

5.8~29.6

Temperature/℃

Performance

Tensile strength/MPa

Elongation/%

RT

1140 ~1210

7.5~13.0

1000

700 ~720

5.2

1200

320 ~360

9.0

1300

190 ~210

11.5 ~13.5

1400

140 ~170

11.0 ~16.0

High temperature tensile strength and elongation

© Copyright 2025 Baoji Toyar Metal Co., Ltd.
Email: info@toyar-yori.com
Address: Baoji High-tech Development Zone, Baoji,China

Product Center
Service and Support
Warehouse: US,Russia,Germany,India,Thailand
Powered by Feedback Manage